PSG Deposition
2008-05-22
Rana, Mukti M
2008-05-23
Glenn Silveira
2008-05-23
乔大勇
PSG Deposition
Glenn Silveira
2008-05-23
If it is a sacrificial layer PECVD undoped TEOS can be deposited that thick

Best regards,
Glenn

-----Original Message-----
From: Rana, Mukti M [mailto:[email protected]]
Sent: Thursday, May 22, 2008 12:43 PM
To: [email protected]
Subject: [mems-talk] PSG Deposition

Hi,

We require to deposit 10.5 um thick PSG for using as a sacrificial layer
by LPCVD. Can anyone tell me about the available foundry services for
this? If you are a vendor please contact me directly. Thank you.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.