PDMS glue recommandation
Philip D. Hewes
2008-05-29
Hong,

I personally use  Dow-Corning 734 silicone sealant/adhesive and it
works great for attaching PDMS to platinum-cured silicone tubing, so I
am sure that it will work well for PDMS-PDMS bonding. It is also a
PDMS-based polymer, so less concern for biocompatibility...

Philip D. Hewes
Department of Biomedical Engineering (Undergraduate)
University of Michigan: School of Engineering
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
University Wafer
Harrick Plasma, Inc.