Selective etching between Cu and Ni / Ag
Ravi Shankar
2008-05-29
Hi Sardar Bilal,

       Cu is the seed layer on wafer and whether Ni and Ag are in
contact with each other (and with Cu)...If the metal layers are in
contact with each other then it may lead to galvanic corrosion in
which one metal corrodes preferentially than the other type of metal
and both metals are in an electrolyte. if this is the case, then you
can try selective metal deposition instead of depositing on whole
wafer and etching later...

-Ravi Shankar
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.
Addison Engineering