I am facing water leakage problem from the copper backing plate of the
sputtering machines, I have tried to seal with many makes and brands of
sealant, but does not works, can any advice me right sealant for sealing the
water leakage ( it is for stop gap measure, till we get a new set of backing
plates )

Regards

Nataraj Santhanam