MEMSnet Home: MEMS-Talk: Dissolving carboxylate modified micro spheres stick to the PDMS channel walls
Dissolving carboxylate modified micro spheres stick to the PDMS channel walls
2008-06-04
Mohammed Asfer
2008-06-04
Le Cao Hoai Nam
Dissolving carboxylate modified micro spheres stick to the PDMS channel walls
Mohammed Asfer
2008-06-04
Dear all

    I am using carboxylate modified micro spheres(1.0 um, nile red
    fluorescent, Invitrogen, molecular probes) for microPIV
    measurements for flows through the microchannel made of PDMS. But
    during flow, some of the the above fluorescent microspheres stick
    to the walls of the PDMS channel. As a result it becomes
    difficult to reuse the above channel. So can anyone tell me what
    solvents can be used to dissolve those particles from the channel
    walls without any changes in the microchannel features.

    Thanks in advance for those who will reply.
--
With regards & Best wishes

Mohammed Asfer
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Harrick Plasma, Inc.
Addison Engineering