A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: 20um features using AZP4620
20um features using AZP4620
2008-06-03
Haixin Zhu
2008-06-04
李加东
2008-06-04
Haixin Zhu
2008-06-04
Robert Black
2008-06-04
Haixin Zhu
2008-06-13
Brubaker Chad
2008-06-13
Haixin Zhu
2008-06-15
Tolga YELBOGA
2008-06-16
Oakes Garrett
2008-06-04
Tolga YELBOGA
2008-06-04
Haixin Zhu
20um features using AZP4620
Haixin Zhu
2008-06-04
We can have the desired thickness, but after the developping(the developping
time is longer than 10mins), the 10um feature is gone and other bigger feature
get little distorted. I believe there are something wrong with the baking and
exposure, but not very clear which one need to be fine-adjusted or corrected.

Any comments

Michael

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of 李加东
Sent: 2008年6月3日 17:10
To: [email protected]
Subject: Re: [mems-talk] 20um features using AZP4620

you can use spray coating

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
The Branford Group
Mentor Graphics Corporation