A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: 20um features using AZP4620
20um features using AZP4620
2008-06-03
Haixin Zhu
2008-06-04
李加东
2008-06-04
Haixin Zhu
2008-06-04
Robert Black
2008-06-04
Haixin Zhu
2008-06-13
Brubaker Chad
2008-06-13
Haixin Zhu
2008-06-15
Tolga YELBOGA
2008-06-16
Oakes Garrett
2008-06-04
Tolga YELBOGA
2008-06-04
Haixin Zhu
2008-08-06
Pradeep Dixit
20um features using AZP4620
Haixin Zhu
2008-06-04
Thanks, Robert,

My main concern is that the bigger pattern (>200um) are distored, with =
clear undercut and edge distortion, any comments on this?

Thanks

Michael

________________________________

From: [email protected] on behalf of Robert Black
Sent: Wed 6/4/2008 2:36 PM
To: 'General MEMS discussion'
Subject: Re: [mems-talk] 20um features using AZP4620

I haven't worked with the P4000 series resist, but in your earlier =
message
you said you we coating at 38um. According to some literature I have =
from
AZ, the max aspect ratio for this resist at 2:1 so 10um features will
probably be gone.

Robert
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing