    It depend on the wafer's doping concentration.If the doping concentration is
high,you can get ohmic contact;otherwise,it's hard to get ohmic contact.
    I usually use Al to get ohmic contact.Process is as follow:
   1)Deposition Al
   2)Lithograhy
   3)Etch Al
   4)Remove PR
   5)Alloying


2008-06-18

xudehui0108

发件人: Moshe
发送时间: 2008-06-17  20:37:23
收件人: General MEMS discussion
抄送:
主题: [mems-talk] Ohmic contact

Hello !
How I can get ohmic contact?
I talk about N type silicon with antimony contamination.
What the optimal metal and the process  to get ohmic contact between the metal
and the silicon   ?

Thank You
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review