A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Polymer residual about RIE etching of SiO2 by CHF3
Polymer residual about RIE etching of SiO2 by CHF3
2008-06-19
liuxf
2008-06-20
Kvel Bergtatt
2008-06-21
Andrew Sarangan
2008-06-23
Kvel Bergtatt
2008-06-25
liuxf
Polymer residual about RIE etching of SiO2 by CHF3
liuxf
2008-06-19
Hi all:

I am currently trying to open a 3um*3um hole via SiO2 with CHF3 RIE etching so
that metal electrode can be deposited via this hole.
But after the metal deposition, it is open circuit. Probably there is some
polymer residual in the hole. Any boday can tell me is there any good way to
remove this? Is oxygen plasma ok? If so, how about the power? Will the oxygen
plasma damage the SiO2? Is there any other reason for this open circuit?

Thank you so much
xinfei

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Addison Engineering
The Branford Group