A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Critical Dry
Critical Dry
2008-06-26
Ramakrishna Kotha
2008-06-26
Shay Kaplan
2008-06-26
Bill Moffat
2008-06-26
Yianni Tousimis
2008-06-26
Kagan Topalli
2008-07-01
Jack Mulligan
2008-07-01
Robert Bock
2008-07-17
ilan yutsis
Critical Dry
Jack Mulligan
2008-07-01
Rama -

Since water is not miscible in acetone what is most likely happening inside
what I assume is an atmospheric dryer is the acetone vapor is leaving the
surfaces at a much faster rate leaving the water behind on the surfaces to
evaporative dry which leaves watermarks or spots which can cause striation
problems.

We have a solution for this using our proprietary vacuum process. Feel free
to write me for more information. I am careful not to put too much
information in an email that might be seen as using the discussion board for
commercial purposes.

Thanks.

Jack Mulligan
HyperFlo
[email protected]


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Ramakrishna Kotha
Sent: Thursday, June 26, 2008 12:34 AM
To: [email protected]
Subject: [mems-talk] Critical Dry

Hi,

I am performing critical dry to release a parallel plate structure, which
has SiO2 as a sacrificial layer

After removing the sacrifical layer-SiO2 with BOE, then the device is
transffered to DI Water and then to Acetone in the critical dry chamber.
After performig critical dry process using Polaron-CPD 7501 tool, all the
structures are damaged (due to stiction problem).

Can anyone, suggest me the accurate process to perform critical dry.

Thanks in advance
Rama
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing