PDMS to PDMS oxygen plasma bonding
Liang Zhao
2008-07-04
yes, it works

2008/7/2 Joshua Tice :

> Hi Jose,
>
> Yes, although in my experience, it doesn't always work as consistently.  I
> always heat my devices afterward to improve the seal (usually 65 C for an
> hour).
>
> When sealing PDMS to PDMS, you can also use different ratios of curing
> agent
> in each layer to create a seal.  See Quake et al.'s paper:
> http://www.sciencemag.org/cgi/content/full/288/5463/113
>
> Josh

--
赵亮
南京大学化学化工学院
Liang Zhao
School of Chemistry and Chemical Engineering, Nanjing University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.
Nano-Master, Inc.