A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Islands found during SU-8 soft-bake
Islands found during SU-8 soft-bake
2008-07-02
郑瑞麟(Ruilin Zheng)
2008-07-03
Gareth Jenkins
2008-07-04
郑瑞麟(Ruilin Zheng)
2008-07-07
Nodes Norbert
2008-07-08
郑瑞麟(Ruilin Zheng)
2008-07-08
Nodes Norbert
2008-07-09
Oakes Garrett
2008-07-14
郑瑞麟(Ruilin Zheng)
Islands found during SU-8 soft-bake
Nodes Norbert
2008-07-07
There could be also a different reason for these islands.
What does the bake module look like?
Is the volume between wafer and bake module cover very low?
It can happen that the solvent condenses inside the bake module at cold spots
and create droplets. Then, these solvent droplets can drip down on the wafer and
cause the islands.
It seems the bake module can handle the solvent fume volume with 2" wafers. But
with 4" wafers, there is too much of it.

First approach to solve this increasing the bake module's exhaust rate.

Best regards,
Norbert Nodes

E-Mail: [email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of ???(Ruilin Zheng)
Sent: Mittwoch, 02. Juli 2008 16:48
To: General MEMS discussion
Subject: [mems-talk] Islands found during SU-8 soft-bake

Hello, everyone,

I've got a problem with SU-8 soft-bake as I shift from 2inch silicon wafer to
4inch: some islands form on the surface during soft bake ( start to appear
at 65 Celsius degree, and remain after 95 Celsius baking ). Does this
problem have something to do with contamination on wafer?
At first, I thought it was caused by uneven solvent content of SU-8 stored
for two or three weeks in covered beaker. But I also tried the fresh
photoresist, and got the same result.

Does anyone have some ideas with this?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Nano-Master, Inc.
Harrick Plasma, Inc.