MEMSnet Home: MEMS-Talk: TMAH solution photosensitivity
TMAH solution photosensitivity
2008-07-08
Kvel Bergtatt
2008-07-09
Starzynski, John
2008-07-16
Moshe
2008-07-16
Shay Kaplan
TMAH solution photosensitivity
Starzynski, John
2008-07-09
The apparent TMAH etch rate is strongly influenced by the native oxide
on the silicon the Si/SiO2 etch selectivity is about 10,000/1.

-----Original Message-----
From: Kvel Bergtatt [mailto:[email protected]]
Sent: Tuesday, July 08, 2008 12:58 PM
To: General MEMS discussion
Subject: [mems-talk] TMAH solution photosensitivity

Hi all!

i'm wondering if somebody can lead me to the right point where i can
find
evidence, if any of TMAH solutions affected by light. i have observed
different etch rates on poly Si and wondering if light could affect
quaternary amines ability to etch Si.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Nano-Master, Inc.
MEMStaff Inc.