I want use black wax for increase the  protection of thin film nitrure
or oxide in KOH while is produced etching on Silicon.
Thanks

--

Lic. Anahi F. Weinstock

INSTITUTO NACIONAL DE TECNOLOGÍA INDUSTRIAL
CENTRO DE INVESTIGACIÓN Y DESARROLLO EN
TELECOMUNICACIONES, ELECTRÓNICA E INFORMÁTICA

Teléfono (54 11) 4724 6200/6300/6400
Interno 6377
Fax (54 11 ) 4754 5194
[email protected]
0800 444 4004 | www.inti.gov.ar




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Mentor Graphics Corporation
The Branford Group