Hello Everyone,

We are trying to use a low temperature curing "spin-on-glass" material
for a good water barrier.  The ones I found online require temperatures
upwards of 250C.  I was looking somewhere between 75 and 80C.  Can
anyone suggest a suitable material for that?  Thanks in advance!

--
Rajib Ahmed, Ph.D.
Staff Research Engineer
Bay Materials, LLC./ Cantimer, Inc.
3700 Haven Court
Menlo Park, CA 94025-1043
Phone # (650)474-0500 X 313
Fax # (650)474-0599
Email Address: [email protected]
www.baymaterials.com
www.cantimer.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
MEMStaff Inc.
Addison Engineering