Qi Luo
2008-07-16
In our structure, we electroplate Ni on Au substrate. Our process has Alkaline
clean, another step of activation, Ni strike, then Ni plating. For our
application, the adhesion of the plated Ni to Au film is very important. Can we
replace the Ni strike with Au strike, or insert a Au strike before Ni strike to
improve adhesion? Your help would be greatly appreciated.
With kind regards,
Qi Luo



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Mentor Graphics Corporation
Harrick Plasma, Inc.