A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Critical Dry
Critical Dry
2008-06-26
Ramakrishna Kotha
2008-06-26
Shay Kaplan
2008-06-26
Bill Moffat
2008-06-26
Yianni Tousimis
2008-06-26
Kagan Topalli
2008-07-01
Jack Mulligan
2008-07-01
Robert Bock
2008-07-17
ilan yutsis
Critical Dry
ilan yutsis
2008-07-17
Hi
In order to do CPD after Si etch in BOE my recipe is as follows:
1. after BOE put in DI water for 5min
2. DI water for 5min
3. ethanol and water 1:1 for 5min
4. ehtanol and water 3:1 for 5min
5.  pure ethanol for 5min
6. pure ethanol for 5min and transfer to CPD
each step in different beeker
Ilan
----- Original Message -----
From: "Jack Mulligan" 
To: "'General MEMS discussion'" 
Sent: Tuesday, July 01, 2008 8:51 PM
Subject: Re: [mems-talk] Critical Dry


> Rama -
>
> Since water is not miscible in acetone what is most likely happening
> inside
> what I assume is an atmospheric dryer is the acetone vapor is leaving the
> surfaces at a much faster rate leaving the water behind on the surfaces to
> evaporative dry which leaves watermarks or spots which can cause striation
> problems.
>
> We have a solution for this using our proprietary vacuum process. Feel
> free
> to write me for more information. I am careful not to put too much
> information in an email that might be seen as using the discussion board
> for
> commercial purposes.
>
> Thanks.
>
> Jack Mulligan
> HyperFlo
> [email protected]
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
MEMS Technology Review
Nano-Master, Inc.