MEMSnet Home: MEMS-Talk: Gold Etchant with selectivity over Mo
Gold Etchant with selectivity over Mo
2008-07-21
Chong Xie
2008-07-23
Moshe
2008-07-23
Kevin Paul Nichols
Gold Etchant with selectivity over Mo
Chong Xie
2008-07-21
Hello everyone,

I am looking for some etchant that can etch away Au and leave Mo. I tried
KI/I2, but it seems it etched Mo as well.

Any input is appreciated, and thanks in advance.

--
Chong Xie
Ph. D Candidate
Cui Group
The Geballe Laboratory for Advanced Materials
476 Lomita Mall, Stanford University
Stanford, CA 94305

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.