MEMSnet Home: MEMS-Talk: Si Etch Initiation Failure
Si Etch Initiation Failure
2008-07-26
Muk Mei Yu
2008-07-26
Kvel Bergtatt
2008-07-27
Shay Kaplan
2008-07-28
Muk Mei Yu
2008-07-28
Muk Mei Yu
2008-08-03
Kvel Bergtatt
Si Etch Initiation Failure
Muk Mei Yu
2008-07-26
Hi,

Did anyone encounter 'etch initiation' failure for Si etch in TMAH solution
before? Some refer etch initiation failure as passivation of Si during etching
which prohibits etching of Si. Si presents un-etched after the whole process.
What are the casues of this phenomenon? Any measures to help mitigate this
defect?

Thanks,
Muk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing