MEMSnet Home: MEMS-Talk: Si Etch Initiation Failure
Si Etch Initiation Failure
2008-07-26
Muk Mei Yu
2008-07-26
Kvel Bergtatt
2008-07-27
Shay Kaplan
2008-07-28
Muk Mei Yu
2008-07-28
Muk Mei Yu
2008-08-03
Kvel Bergtatt
Si Etch Initiation Failure
Kvel Bergtatt
2008-07-26
Try a oxide etching as a pre-step; native oxide and organic junk inhibits Si
etching; also make sure to use a dilute TMAH solution, hight temperature and
sonication if possible.

On Fri, Jul 25, 2008 at 10:18 PM, Muk Mei Yu  wrote:

> Hi,
>
> Did anyone encounter 'etch initiation' failure for Si etch in TMAH solution
> before? Some refer etch initiation failure as passivation of Si during
> etching which prohibits etching of Si. Si presents un-etched after the whole
> process. What are the casues of this phenomenon? Any measures to help
> mitigate this defect?
>
> Thanks,
> Muk

--
_fm
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.