MEMSnet Home: MEMS-Talk: Su 8 thickness
Su 8 thickness
2008-08-06
jiang Liudi
2008-08-06
Wei Cheng
2008-08-07
jiang Liudi
2008-08-08
eowin rohan
2008-08-06
jiang Liudi
2008-08-06
Oakes Garrett
2008-08-07
jiang Liudi
2008-08-08
Oakes Garrett
2008-08-12
jiang Liudi
2008-08-13
Oakes Garrett
Su 8 thickness
Oakes Garrett
2008-08-08
Hi,

When I do double coats of SU-8 to 100 or 150 µm I simply perform the same coat
sequence twice.  Thicker double coats may require changes to the first bake
process.  Excessive heat seems to begin crosslinking SU-8 at the wafer but that
shouldn't be the case here.

Best Regards,
Garrett Oakes

EV Group
invent * innovate * implement
Regional Sales Manager North America - Direct: +1 (480) 305 2443, Main: +1 (480)
305 2400 Fax: +1 (480) 305 2401
Cell: +1 (480) 516 6724
E-Mail: [email protected], Web: www.EVGroup.com

-----Original Message-----
From: jiang Liudi [mailto:[email protected]]
Sent: Thursday, August 07, 2008 12:27 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Su 8 thickness

Hi,
Many thanks for kind suggestions.

I think double coat could be the solution. could you further suggest procedures
of double layers in terms of baking, expose and PEB?According according to the
data sheet, 1700rpm should get almost 140um thickness. is it common for half the
thickness, compared with the sheet?

thanks again.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics