A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photolithography - Resist peeling
Photolithography - Resist peeling
2008-08-15
madhav rao
2008-08-15
Abhishek Jain
2008-08-17
Suraj Patil
2008-08-15
[email protected]
2008-08-15
SEBESTA Edward
2008-08-15
Jon R. Fox
2008-08-15
Bill Moffat
2008-08-15
Andrea Mazzolari
2008-08-15
Bruce Neufeld
2008-08-16
Kvel Bergtatt
2008-08-16
Michael Larsson
2008-08-18
Michael Larsson
Photolithography - Resist peeling
madhav rao
2008-08-15
Hi,
       I am experiencing a problem in patterning on silicon-di-oxide wafers; I
am using SHIPLEY 1818 resist to get a thickness of 2.5 micron; 6 seconds of
exposure time. After developing for 60 seconds, I observe, the resist layer
peels off; leaving no patterns on the wafer. Also I had soft-baked the resist at
95 C for 2 minutes in hot-plate.
This seems strange to me, as a month ago, I had successfully transferred the
patterns on to silicon-di-oxide wafers.
I am using mylar film masks.
Please let me know, if any one had experienced similar problems before; and if
so, could you let me know suggestions to solve ?

Thanks

Regards,
Madhav Rao,
Graduate student,
University of Alabama.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review