A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photolithography - Resist peeling
Photolithography - Resist peeling
2008-08-15
madhav rao
2008-08-15
Abhishek Jain
2008-08-17
Suraj Patil
2008-08-15
[email protected]
2008-08-15
SEBESTA Edward
2008-08-15
Jon R. Fox
2008-08-15
Bill Moffat
2008-08-15
Andrea Mazzolari
2008-08-15
Bruce Neufeld
2008-08-16
Kvel Bergtatt
2008-08-16
Michael Larsson
2008-08-18
Michael Larsson
Photolithography - Resist peeling
Bill Moffat
2008-08-15
Variations are caused by variations in atmospheric humidity.  Vacuum
vapor prime.  Vacuum dehydrates totally.  HMDS vapor reacts with
Hydroxyl ions on wafer and creates an inorganic molecule/organic
molecule bridge. Perfect resist adhesion always.

Bill Moffat
________________________________

From: [email protected] on behalf of madhav rao
Sent: Fri 8/15/2008 10:39 AM
To: [email protected]
Subject: [mems-talk] Photolithography - Resist peeling

Hi,
       I am experiencing a problem in patterning on silicon-di-oxide =
wafers; I am using SHIPLEY 1818 resist to get a thickness of 2.5 micron; =
6 seconds of exposure time. After developing for 60 seconds, I observe, =
the resist layer peels off; leaving no patterns on the wafer. Also I had =
soft-baked the resist at 95 C for 2 minutes in hot-plate.
This seems strange to me, as a month ago, I had successfully transferred =
the patterns on to silicon-di-oxide wafers.
I am using mylar film masks.
Please let me know, if any one had experienced similar problems before; =
and if so, could you let me know suggestions to solve ?

Thanks

Regards,
Madhav Rao,
Graduate student,
University of Alabama.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Addison Engineering
Mentor Graphics Corporation