A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Gas Phase Lubricant
20um features using AZP4620
2008-08-06
Pradeep Dixit
Gas Phase Lubricant
2008-08-19
Jian Wang
2008-08-19
Bill Moffat
Silanizing a Glass Microchannel
2008-08-20
Kevin Paul Nichols
2008-08-21
Bill Moffat
Gas Phase Lubricant
Jian Wang
2008-08-19
Dear all,

I am working on PDMS microdevice. I need to lubricate the moving parts in
the microchannels (200 um). Any suggestion about gas phase lubricant for
microchannels?

Appreciate your help.

Jian