Hello all,

I was doing some research of bonding two initially aligned Si pieces.
A homemade thermal bonder has been used, which can provide force
and heat the samples. However, due to the shear force generated by
the bonder head on the samples, the initial alignment was broken
during the bonding. Is there any way that I can reduce the shear force
to avoid breaking the alignment? Any suggestion is appreciated.

Thanks,
Lin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Mentor Graphics Corporation