A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Positive Resist Development Mechanism
Positive Resist Development Mechanism
2008-09-02
[email protected]
2008-09-03
Brad Cantos
2008-09-04
Richard B. Keithley
2008-09-04
[email protected]
2008-09-03
Shay Kaplan
2008-09-03
[email protected]
2008-09-03
Bill Moffat
2008-09-04
[email protected]
2008-09-04
Brad Cantos
Positive Resist Development Mechanism
Richard B. Keithley
2008-09-04
Here is a very good (but old) resource.  It describes mechanisms and
then some.  It is an all around good reference, has some good advice
about resists, but the technology is a bit outdated now.

Thompson, L.F., C.G. Wilson, and M.J. Bowden,
Introduction to Microlithography: Theory, Materials,
and Processing. ACS Symposium Series. Vol. 219.
1983, Washington, D.C.: American Chemical Society.

ISBN:  0841207755

-R

Richard B. Keithley
UNC Analytical Chemistry Graduate Student &
National Defense Science and Engineering Graduate Fellow
Wightman Research Group
Chapel Hill, NC 27599
919-962-1108

Brad Cantos wrote:
> Have you tried doing a brief descum or surface plasma etch prior to
> developing?  In the past when I used an iodine solution to etch
> electroplated gold this usually helped.
>
> Brad Cantos
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Addison Engineering