Dazhong,

All it sounds like they're describing is dissolving some PMMA in acetone
(which it's readily soluble in), then placing a few droplets of that on a
glass slide and letting it evaporate. It could be done with something as
simple as a pipette. It won't be very uniform, but it will be a film of
PMMA.

- Kevin

> From: Dazhong Wu 
> Organization: Illinois Institute of Technology
> Reply-To: General MEMS discussion 
> Date: Mon, 08 Sep 2008 23:42:00 -0600
> To: mems-talk 
> Subject: [mems-talk] How to prepare PMMA films
>
> Hi there,
>
> Does anyone have experience of depositing PMMA on glass slide to prepare PMMA
> films?
> I got the following information in a reference:
> " depositing droplets of 10g of PMMA in 15g of acetone on glass slide and
> letting acetone evaporate over a few days"
>
> But what exact deposit method should I use? what instrument should I use? I
> have no this kind of knowledge before, So I appreciate someone can tell me the
> details.
>
> Sincerely,
> Dazhong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
University Wafer
Tanner EDA by Mentor Graphics