MEMSnet Home: MEMS-Talk: How to get homogeneous surface by isotropic wet etch ?
How to get homogeneous surface by isotropic wet etch ?
2008-09-15
Moshe
How to get homogeneous surface by isotropic wet etch ?
Moshe
2008-09-15
Hi

when I operate  isotropic wet  etch ( HNO3:HF - 98:2 ) for silicon piece the
thickness at the edge is thin from the center.

I am looking for solution to get homogeneous surface all over the piece.

Thank you, Moshe