I need to etch 5 microns of sacrificial PECVD SiO2 using isotropic plasma
etch. Does anyone have any experience with this? I have seen that in
literature CF4 is mentioned to be isotropic plasma but not too many details.
Any extra info will is welcome.

Sincerely yours,

Sebastian Sosin
Yahoo Messenger: sosin_sebastian
Address: Delft University of Technology, Mekelweg 4, Room LB 01.380
2628 CD DELFT, the Netherlands
Mobile Phone #:  +31(0)651976932
Office Phone #:  +31(0)152789421

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
The Branford Group
MEMStaff Inc.