Sebastian Sosin
2008-10-06
SEBESTA Edward
2008-10-07
Morten Aarøe
SiO2 isotropic plasma etch
SEBESTA Edward
2008-10-06
I see some problems with this.

1. CF4 will have difficulty in etching SiO2. The stoichiometry is unbalanced.

2. The anistropic or isotropic nature of a plasma etch is driven by the
substrate to plasma bias and not the chemistry.

3. When SiO2 is etched with CHF3 or something with a lower F:C ratio, it needs
an Reactive Ion Etch where there is a carbon residue and bombarment of this
residue by use of a bias to drive a Carbon oxygen reaction to facilitate the
etching of SiO2. This is inherently anisotropic.

4. If you need to etch isotropically 5 microns, I would use a wet etch solution
which is inherently isotropic.

Ed

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Sebastian Sosin
Sent: Monday, October 06, 2008 4:00 AM
To: [email protected]
Subject: [mems-talk] SiO2 isotropic plasma etch


I need to etch 5 microns of sacrificial PECVD SiO2 using isotropic plasma etch.
Does anyone have any experience with this? I have seen that in literature CF4 is
mentioned to be isotropic plasma but not too many details.
Any extra info will is welcome.

Sincerely yours,

Sebastian Sosin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
The Branford Group
MEMStaff Inc.