Questions regarding silane coating and surface cleaning
김태진
2008-10-06
Hi!

I'm trying to treat Silicon wafers or PDMS with Silane to make it hydrophobic.
As far as I recall, all I need is a dessicator.

But someone told me that I need a plasma asher for it.
Is this true? How exactly do I coat Silane on surfaces?

Also, I'm trying to purchase a cost effective plasma system for Silicon, glass
and PDMS surface cleaning.

My second question is: is a microwave type oxygen plasma system good enough for
surface cleaning?

Thank you!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
The Branford Group
Addison Engineering