I tried this. You should do some silane chemistry on the SiO2 surface to promote
parylene adhesion (see e.g.
http://engineering.tufts.edu/microfab/index_files/docs/Parylene.pdf).
Even then, it doesn't work too well, the parylene tended to delaminate during
long etch cycles.

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Konstantin Glukh
Sent: Tuesday, October 07, 2008 4:30 PM
To: General MEMS discussion
Subject: [mems-talk] Parylene mask for KOH etch

Can anyone comment on using Parylene as a mask for KOH etch, either by
itself or in addition to SiO2 hardmask? Is there any way to ensure
good adhesion to Si and SiO2 and minimize undercut rate?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review