Filling deep vias with resist
2008-10-27
Black, Robert
2008-10-28
Suzanne Scullen Ericson
2008-10-28
Jan Newman
2008-10-28
Robert Black
2008-10-28
Kevin Paul Nichols
2008-10-29
Michael D Martin
2008-10-29
汪飞
2008-10-27
[email protected]
Filling deep vias with resist
Black, Robert
2008-10-27
     I'm trying to fill some deep vias (25um wide, 70um deep) with resist. I
can't seem to get the resist to go any deeper than about 40um. The best results
were with using a PGMA pre-wet.  I've tried some 55cp resist that I coated three
times to fill (based on top down zygo) and some 120 cp resist. X-sections show
both resists to only be 40um down the vias.
    Any suggestions?

Robert
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.