A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Filling deep vias with resist
Filling deep vias with resist
2008-10-27
Black, Robert
2008-10-28
Suzanne Scullen Ericson
2008-10-28
Jan Newman
2008-10-28
Robert Black
2008-10-28
Kevin Paul Nichols
2008-10-29
Michael D Martin
2008-10-29
汪飞
2008-10-27
[email protected]
Filling deep vias with resist
Jan Newman
2008-10-28
Hi Robert,

         Do you need to fill them or merely protect the internal surfaces?
If only protection required the EVG Nanospray will do the job.
If you need to fill them then the spray can act to initially wet the
internal surfaces and help fill during coating.

Jan

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Black, Robert
Sent: 27 October 2008 15:04
To: [email protected]
Subject: [mems-talk] Filling deep vias with resist

     I'm trying to fill some deep vias (25um wide, 70um deep) with resist. I
can't seem to get the resist to go any deeper than about 40um. The best
results were with using a PGMA pre-wet.  I've tried some 55cp resist that I
coated three times to fill (based on top down zygo) and some 120 cp resist.
X-sections show both resists to only be 40um down the vias.
    Any suggestions?

Robert
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing