MEMSnet Home: MEMS-Talk: LPCVD silicon nitride etch
LPCVD silicon nitride etch
2008-10-28
Deepasree Konduparthi
2008-10-28
Xiaoguang Liu
2008-10-30
Deepasree Konduparthi
2008-10-30
SEBESTA Edward
LPCVD silicon nitride etch
SEBESTA Edward
2008-10-30
 One thing to try is to just use CF4, and monitor the emission lines.
When your N or CN line vanishes  do a brief over etch.

You might have a mixture of CF4 and CHF3 to make sure you get an
appreciable CN emmission.

I am thinking that you have a series of SiO2, Si3N4, Si and so you need
some intermediate chemistry that will etch Si3N4 but will chock
stoichiometrically on Si.

However, that might be making this into too much of a project and you
can just use an emission line monitoring to endpoint when the etch
reaches the Si under the Si3N4.

Ed
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
University Wafer