A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Is three is differences between BOE and HF solution (10-48%) for etching native oxide layer?
Is three is differences between BOE and HF solution (10-48%) for etching native oxide layer?
2008-11-12
Moshe
2008-11-13
Mantavya Sinha
2008-11-13
James Paul Grant
2008-11-14
汪飞
2008-11-14
James Paul Grant
2008-11-14
Christopher Tan
Is three is differences between BOE and HF solution (10-48%) for etching native oxide layer?
汪飞
2008-11-14
Dear James,

"Obviously HF etching is isotropic (etches in all directions) so to reduce
the undercut of patterned features one should choose an BOE concentration
and etch time accordingly."

I think BOE etching is also isotropic. So, why do you think it can help with
better undercut profile?

2008/11/13 James Paul Grant 

> Hello Moshe,
>
> Perhaps this is a simplistic view however the major difference between BOE
> and 49% HF is their etch rate.
>
> 49% HF will etch much faster than 5:1 BOE which in turn will etch much
> faster than 10:1 BOE. Might I suggest you have a look at the (in my view)
> excellent paper, "Etch Rates for Micromachining Processing -Part II" by Kirt
> Williams (Journal od Micromechanical systems Vol. 12, No. 6 December 2003).
>
> The native oxide on silicon is only 20 A thick and 10: 1 BOE will remove
> native oxide at around 20 nm/minute so I would use this BOE for around 30
> seconds.
>
> Obviously HF etching is isotropic (etches in all directions) so to reduce
> the undercut of patterned features one should choose an BOE concentration
> and etch time accordingly.
>
> James

--
Best regards,
Yours sincerely
Fei Wang
______________
Postdoctoral researcher, Dr
MIC - Department of Micro and Nanotechnology
Technical University of Denmark (DTU)
Building 344, 1st floor, Room no. 130
DK-2800, Kgs. Lyngby
Denmark
Tel:  +45 4525 6311
Fax:  +45 4588 7762
Email: fei.wang@nanotech.dtu.dk
      http://www.nanotech.dtu.dk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing