Cu electroplating uniformity problem
2008-11-18
Denis Petrov
2008-11-18
Robert Bock
2008-11-18
李加东
2008-11-19
Shay Kaplan
2008-11-19
Kuijpers, P e m
Cu electroplating uniformity problem
李加东
2008-11-18
My research is about the uniformity control of electroplating.

There's one conclusion of my research paper:

The uniformity and profiles of electroplated nickel
posts are controlled mainly by plating current density
and temperature. Optimal conditions of 8.05mA/cm2 and
20°C were obtained to fabricate flat cross-sectional
profile microstructures and a uniform thickness
distribution across a specimen.


--

联系方式:
地址:长春经济技术开发区东南湖大陆16号应用光学国家重点实验室微机械组
邮编:130033
联系电话:0431-86176918(office)0431-86176544(home) 13644300593(phone)



在2008-11-18,"Denis Petrov"  写道:
>Hello dear MEMS-Talk members!
>
>We are trying to electroplate 20-um thick copper over patterned 4-inch wafers.
>The problem is the uniformity of the Cu layer. If it is approx. 20 um
>in the middle of the wafer then we have something like 25 um at the
>edges.
>
>I found out that there is a device called an IBM Paddle Cell. Does
>anybody know anything about it? Is it of help in this case? Is there
>any other practical solution.
>We tried the rotating cathode method and we tried to agitate the
>solution with the rotating paddle. Did not help.
>
>Thank you!
>
>--
>M.Sc. Denis Petrov
>Ph.D. Student
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Mentor Graphics Corporation