A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SiO2 deposition
SiO2 deposition
2008-11-21
[email protected]
2008-11-21
SEBESTA Edward
2008-11-21
John Hilton
2008-11-21
SEBESTA Edward
2008-11-23
Konstantin Glukh
2008-11-23
Tom Rust
2008-11-24
Juergen Leib - GMX
SiO2 deposition
SEBESTA Edward
2008-11-21
I think you probably have a silicon suboxide and defects, but I would
think that an O2 anneal would solve the problem. Even at 900 deg. C or
maybe less.

Ed

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of John Hilton
Sent: Friday, November 21, 2008 1:27 PM
To: General MEMS discussion
Subject: Re: [mems-talk] SiO2 deposition

I recently had OK results depositing a film of 2-3 microns SiO2 using an
e-beam evaporator.  The stoichiometry probably isn't exactly right, and
this was backed up by the fact that the dielectric strength didn't seem
as good as it should be (probably too much pure Si).  I haven't tried a
layer as thick as 20-30 microns.  What is your application?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Nano-Master, Inc.