MEMSnet Home: MEMS-Talk: Re: A. low stress Si3N4 in PECVD ?
Re: A. low stress Si3N4 in PECVD ?
1998-09-28
Lionel Buchaillot
1998-09-28
[email protected]
1998-09-28
Shile
Re: A. low stress Si3N4 in PECVD ?
Lionel Buchaillot
1998-09-28
One recent reference is:
Resisual stress in low pressure chemical vapor deposition SiNx films
deposited from silane and ammonia
P. Temple-Boyer et al.
J. Vac. Sci. Technol. A 16(4), Jul/Aug 1998 2003-2007

lee ki seong wrote:
>
> Hi. colleague
>
> Is any body know how we can get low stress Si3N4 in PECVD using SiH4, NH3
>    RF POWER, Temp, Pressure, Vacuum.
>
> If some body has a trend to lessen the stress, would you inform me ?
>
> with thanks.
>

--
********************************************
Lionel BUCHAILLOT
Microsystemes Silicium
Silicon Microsystems
IEMN Departement ISEN
Cite Scientifique
Avenue Poincare - B.P. 69
59652 VILLENEUVE D'ASCQ Cedex
FRANCE

E-mail : [email protected]

Phone : +33 3 20 19 78 38
Fax : +33 3 20 19 78 84
********************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.