A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Question about perforation
Question about perforation
2008-11-27
Yan Xin
2008-11-28
matthew king
2008-11-28
Morten Aarøe
2008-11-28
汪飞
2008-11-29
Yan Xin
2008-11-29
Jie Zou
2008-11-30
matthew king
2008-11-29
mrutyu swamy
Question about perforation
matthew king
2008-11-30
Mr Yan,

    Sorry. The dimension calculation in last message is wrong.

    From my understanding, undercut refers to the difference betweeen oxide and
silicon. That is, if the silicon hole size is 10um, then the oxide hole size
will be 10+1.8*2=13.6 um.

                                          Matthew King



> Hi everyone,
>
> For the inertial sensors, we usually need to perforate the
> suspended
> structure to release the structure with wet etching
> process.
> -But how to know if the holes are big or dense enough to
> release the structure
> completely?
>
> For example, in the SOIMUMPs process, the oxide layer is 1
> microm, the
> structure layer is about 25 micron, undercut is 1.8 micron
> per side by  HF
> vapor etching,
> -Does this mean that  the distance between edges of  two
> adjacent etched
> holes must be less the 1.8*2 micron if i need  to release
> the structure
> completely?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing