A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Stress reduction in SOI
Stress reduction in SOI
2008-12-15
Jason Milne
2008-12-15
Andrea Mazzolari
2008-12-16
Jason Milne
2008-12-15
Michael
2008-12-16
[email protected]
2008-12-19
Trent Huang
Stress reduction in SOI
[email protected]
2008-12-16
Hi Michael, the devices are single layer structures, and they should
not have an oxide layer: the observation of buckling and curvature was
made immediately (2 mins) after the SiO2 etch to release the
structures (15 mins in 50% HF), which would have stripped any oxide.
The process was entirely based on photoresist masking and wet etching,
so I don't think it can be any other layer causing the stress issues.

Jason Milne


Quoting Michael :

> Hi Jason
>
> Do you have any oxide layer on your micro-bridge or cantilever devices?
> Are they a single layer structures? It is important that you are
> sure you made the structures out of the device layer only.
> regards,
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics