Au electroplating on Al substrate
2009-01-07
Denis Petrov
2009-01-07
Alexandre BOE
2009-01-07
Oakes Garrett
2009-01-08
Ravi Shankar
2009-01-08
IGOR KADIJA
2009-01-08
Heather Broadbent
2009-01-08
Edward Sebesta
2009-01-08
Wilson, Thomas
2009-01-08
Brad Cantos
2009-01-08
Huihang Dong
Au electroplating on Al substrate
Oakes Garrett
2009-01-07
Denis,

I think that more specific information regarding the process that you are trying
to use is needed to receive better guidance from this group.  In general, you
could be experiencing issues with surface oxide layers that prevent plating or
adhesion of the plated material to the aluminum itself.

I am by no means a plating expert.  That written, the following webpage is a
good reference for plating materials onto aluminum:

        http://www.eaa.net/eaa/education/TALAT/lectures/5105.pdf

Best of luck,
Garrett Oakes

EV Group
invent * innovate * implement
Regional Sales Manager North America - Direct: +1 (480) 305 2443, Main: +1 (480)
305 2400 Fax: +1 (480) 305 2401
Cell: +1 (480) 516 6724
E-Mail: [email protected], Web: www.EVGroup.com

-----Original Message-----
From: Denis Petrov [mailto:[email protected]]
Sent: Wednesday, January 07, 2009 6:16 AM
To: General MEMS discussion
Subject: [mems-talk] Au electroplating on Al substrate

Hi all!

Happy New Year, first of all!

My question is, did anybody try to electroplate gold onto Al surface.
We have tried that at our facility recently. After 15 min. absolutely
nothing happened. No gold at all.

We shall be thankful for any suggestions.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group