Hello. I'm interested in applying a thin (~50 nm) superconducting,
conformal and non-oxide forming coating on Aluminum. Would anyone be
able to provide a reference (or ideally a bath vendor) for electroless
immersion plating of Ruthenium on Aluminum?  Thank you.