MEMSnet Home: MEMS-Talk: hard ashing polymer (if Al deposited): possible isotropic etch by ICP?
hard ashing polymer (if Al deposited): possible isotropic etch by ICP?
2009-01-29
onny setya
2009-01-29
Edward Sebesta
2009-01-30
onny setya
2009-01-30
Edward Sebesta
2009-02-02
onny setya
2009-02-02
Edward Sebesta
2009-01-29
Jie Zou
hard ashing polymer (if Al deposited): possible isotropic etch by ICP?
Jie Zou
2009-01-29
It should be possible if you have a strong enough ICP system. My
understanding is you have a SiO2+Al structure with polymer underneath and
you want to release it.

The first thing you need check is whether your Al layer covers all of your
polymer and how much undercut you need to release your structure. >1um
undercutting may be impossible.

Jie

On Thu, Jan 29, 2009 at 9:23 AM, onny setya  wrote:

>
> Hello everyone,
>
> I'm having difficulty removing the polymer under the dielectric material
> whose Al is around 60nm deposited on it
>
> We have done these steps: on the substrate: ~600nm SiO2 or SiNx are
> deposited; then ~200nm polymer is applied, after that again 600nm SiO2 or
> SiNx layer, and the last is Al ~60-100nm (ebeam evaporation)
>
> I removed completely the polymer, for around 3h, using an asher
> (oxygen-plasma) if the samples don´t have the Al layer on it.  For the same
> ashing process I didn´t get the same result for another sample whoose Al on
> it.
>
> That´s why I would like to know:  does anyone know whether it´s possible to
> get isotropic etching using only oxygen gas (maybe using ICP)?  Or any
> suggestion will be appreciated.
>
> Many thanks!
>
> Onny Setyawati

*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Tel: +1-352-846-8018
*  Email: [email protected]
*  Homepage: http://plaza.ufl.edu/zoujie/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group