MEMSnet Home: MEMS-Talk: Double lithography problem with SU1828-TI35ES
Double lithography problem with SU1828-TI35ES
2009-01-29
basar bolukbas
2009-01-29
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Edward Sebesta
2009-01-30
basar bolukbas
2009-02-02
Edward Sebesta
Double lithography problem with SU1828-TI35ES
basar bolukbas
2009-01-30
Hello Edward.

Which kind of plasma treatments are suitable for SU1828?
Or is it not changeable resist by resist?
I use SU1828 for first lithography and TI35 for second.
I think i will treat SU1828 but i am not sure for the ambient.
I can apply O2 plasma, CHF3, SF6, CCl2 with RIE also.

Which one is suitable do you think?

Thank you for your help.

Best Regards.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.