MEMSnet Home: MEMS-Talk: Looking for mask to make holes in glass
Looking for mask to make holes in glass
2009-03-04
Moshe
2009-03-04
John Dangtran
2009-03-06
Albert Henning
2009-03-04
Mehmet Aykol
2009-03-04
Andrea Mazzolari
2009-03-04
Hanson, Steve
2009-03-06
Zhao Lu
2009-03-09
Mikael Evander
2009-03-05
Moshe
2009-03-05
walter
2009-03-05
Fei Wang
2009-03-06
Morten Aarøe
2009-03-06
Pat Kayatta
2009-03-06
akshdeep sharma
Looking for mask to make holes in glass
Moshe
2009-03-05
Thank you for all the answers
I prefer to focus on a way to made holes with wet etch.
I there a resist so the HF do not strip it ?
As I said I tried gold and polysilicon and the HF strip it.




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing