Philips XL 30 ESEM HTSU Arching Over 10kV
2009-03-11
Qinghong Du
2009-03-12
Brian Stahl
2009-03-12
Qinghong Du
Philips XL 30 ESEM HTSU Arching Over 10kV
Brian Stahl
2009-03-12
Hello Du,

Do you only encounter this arcing issue when running the microscope in
environmental SEM mode?  If so, it probably means your chamber pressure is
too high and the water vapor (or whatever gas you're flowing) is ionizing.
Try reducing the pressure in your chamber.

Good luck,

Brian C. Stahl
Graduate Student Researcher
UCSB Materials Research Laboratory
[email protected] / [email protected]
Cell: (805) 748-5839
Office: MRL 3117A


On Wed, Mar 11, 2009 at 3:30 PM, Qinghong Du  wrote:

> Hi,
>
> We have a Philips XL30 ESEM system. Recently, the system only can work
> under 10kV. Over 10kV, there is arching issue in the HTSU unit. Does anybody
> have this experience and any idea to fix it?
>
> Thanks a lot.
>
> Du
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMStaff Inc.