MEMSnet Home: MEMS-Talk: Anyone have Experience on PDMS patterning
Anyone have Experience on PDMS patterning
2009-03-23
王××
2009-03-23
Hong Chen
Anyone have Experience on PDMS patterning
Hong Chen
2009-03-23
Try photopatternable PDMS

Hong Chen

On Mon, Mar 23, 2009 at 1:58 PM, 王××  wrote:
> I want to make some 50um deep PDMS channels on a glass wafer surface.
>
> However I can't use the typical PDMS process, which includes making master
using SU-8, then pouring PDMS and bonding PDMS with Glass.
>
> Are there any suggestions?
>
> My Idea:
>
> 1. Pattern the channel using negative mask (dark in channel area), use
positive PR (AZ4620)
>
> 2. Spin coat PDMS on top of AZ4620 pattern.
>
> 3. Spin coat AZ4210 or AZ4110 on top of PDMS
>
> 4. Pattern the AZ4210 using positive mask (transparent in channel area)
>
> 5. After exposing the channel area from last step, Use RIE to etch the PDMS
away and expose the AZ4620.
>
> 6. Use Acetone to remove the AZ4620.
>
> My concern is the PDMS might have a climbing effect on step 2, so the PDMS
surface will not be flat.

--
Research Assistant,
Mech. Eng., URI
92 Upper College Rd.,
Kingston, RI 02881

Office Tel : 401-874-2247
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group
Nano-Master, Inc.