li shifeng
2009-04-01
Brad Cantos
2009-04-01
Ruiz, Marcos Daniel (SENCOE)
2009-04-02
Edward Sebesta
2009-04-02
Robert MacDonald
Pin Holes on the Al Surface
li shifeng
2009-04-01
Hi, I used to ebeam to deposit Al on the glass substrate. I found some black
stuffs distributed on the entire Al surface after deposition. Following dry
etching transfer these to the glass substrate and make the surface very rough. I
do not what are these black stuffs and how to get ride of them. Anyone has the
similar experiences and solution.

Thanks!

shifeng
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
Nano-Master, Inc.