UV curable epoxy
2009-04-01
Mehmet Aykol
2009-04-01
Bryan Bishop
2009-04-01
Mehmet Aykol
2009-04-01
Bryan Bishop
2009-04-01
Adamson, Steve
2009-04-01
Mehmet Aykol
2009-04-01
Adamson, Steve
UV curable epoxy
Bryan Bishop
2009-04-01
On Wed, Apr 1, 2009 at 10:59 AM, Mehmet Aykol  wrote:
> Bryan,
> Here is a link to the paper I mentioned.
> http://www.iop.org/EJ/article/0960-1317/16/12/020/jmm6_12_020.pdf?request-
id=61ed6841-6dc8-4bbe-bde4-9923bce89a13
>
> I don't know if you will be able to reach it.

Ah, yeah, I've seen this one before and found some other related
papers- see the following:

http://heybryan.org/books/papers/microfluidics/Bonding%20of%20glass-
based%20microfluidic%20chips%20at%20low-%20or%20room-
temperature%20in%20routine%20laboratory.pdf

http://heybryan.org/books/papers/microfluidics/%20Bonding%20of%20soda-
lime%20glass%20microchips%20at%20low%20temperature%20(65%20celsius).pdf
http://heybryan.org/books/papers/microfluidics/Bonding%20of%20glass-
based%20microfluidic%20chips%20at%20low-%20or%20room-
temperature%20in%20routine%20laboratory.pdf

http://heybryan.org/books/papers/microfluidics/Room%20Temperature%20Microchannel
%20Fabrication%20for%20Microfluidic%20System%20-%20see%20evaporation%20force%20p
aper.pdf
http://heybryan.org/books/papers/Sub-100%20nm%20organic%20light-emitting%20diode
s%20patterned%20with%20room%20temperature%20imprint%20lithography.pdf

Hope this helps.

- Bryan
http://heybryan.org/
1 512 203 0507
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation